Item |
Unit |
AMB |
Ceramic Type | - |
ZTA |
Ceramic Bending Strength |
Mpa |
≥600 |
Ceramic Coefficient of Thermal Expansion(20-600℃) |
ppm/℃ | 6.2 |
Ceramic Thermal Conductivity(25℃) |
W/(m·K) | ≥25 |
Peel Strength(25℃) |
N/mm |
≥10
(0.3mm Cu)
|
Void |
- |
<0.5% |
Insulation Strength(25℃) |
KV/mm |
>20 |
Insulation resistance(25℃) |
Ω |
>1014 |
Thermal Shock(-55℃~150℃) | cycles |
≥300
(0.32mm Ceramic +double 0.5mm Cu)
|